Get in touch

We really appreciate your interest in HORIBA MIRA

Proving Ground Surface

Corrosion Facility

The corrosion facility and the corrosion chamber can be used individually or in combination to accelerate corrosion.

Applications

  • Accelerated corrosion

Salt Splash

  • Single user facility red light signal-controlled approach
  • Housed in an open-ended building
  • Designed for speeds up to 30 mph
  • 35m long x 3.5m wide
  • Walled to provide splashback
  • Brine solution 15 – 20mm deep
  • Solution 4% to 6% by volume, (40 – 60 grams per litre)
  • Spray heads located at the start of the building

Mud Trough

  • Single user facility
  • The trough is walled and 35m long by 5.5m wide
  • Width allows vehicle to zigzag
  • Solution consists of water, sand and loam
  • Sand 4% to 7%
  • Loam 8% to 12%
  • Float controlled water depth of 59mm

Corrosion Facility Description – Salt Flash & Mud Trough.